Hi guys,
I'm rebuilding my 7MGTE, here are the plastigauge results on main bearings:
(mm)
[TD]
0,050
[/TD][TD]
0,070
[/TD][TD]
0,053
[/TD][TD]
0,053
[/TD][TD]
0,070
[/TD][TD]
0,050
[/TD][TD]
0,050
[/TD]TSRM specs in mm:
I use Clevite77 and ARP everywhere, torqued to ARP spec with ARP lube.
Here are rod bearing clearances FYI:
[TD]
0,038
[/TD][TD]
0,040
[/TD][TD]
0,043
[/TD][TD]
0,045
[/TD][TD]
0,045
[/TD][TD]
0,050
[/TD]TSRM specs (mm):
The engine is a 7MGTE I'm building for 600whp (Wisecos, Eagle, MHG, etc..)
What do you think guys for the loose side of mains?
Thanks,
Reynald
I'm rebuilding my 7MGTE, here are the plastigauge results on main bearings:
(mm)
Std Min | Std Max | Grand Max |
0,030 | 0,048 | 0,070 |
Here are rod bearing clearances FYI:
Std Min | Std Max | Grand Max |
0,021 | 0,053 | 0,07 |
What do you think guys for the loose side of mains?
Thanks,
Reynald